Abstract

Roasting pre-treatment is a necessary process for recovering pyrolusite and carbonaceous gold ore. In order to reduce energy consumption and make full use of the carbon component in carbonaceous gold ore, the gold ore was used as the reductant in pyrolusite processing. Based on the fluidized roasting coupling technology, the roasting process of reducing pyrolusite with carbonaceous gold ore was investigated. Co-recovery of manganese from pyrolusite and gold from carbonaceous gold ore was achieved. The results indicated that the optimum leaching efficiency of 99.31 % for manganese and 97.43 % for gold could be attained under the conditions that the mass ratio of carbonaceous gold ore to pyrolusite was 2:3, the co-roasting temperature was 1073.15 K, the roasting time was 30 min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.