Chemical composition, particle size, and structure formation of colloidal Cu 2O and metallic Cu synthesized from Cu(II) acetate in an environmentally friendly 1,2-propane diol were studied dependent on the temperature and concentration of the precursor. Cu 2O as a reaction intermediate is formed between 150 and 170 °C, while its reduction to metallic Cu occurs between 170 and 180 °C. Average particle sizes of non-agglomerated Cu powders varied from 100 nm to 1 μm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.