Abstract

Permanently increasing in the amount of sludge resulted in the serious environment burden. This work reports a novel carbothermal process for converting the Fe-rich waste sludge into cleaner nano-flake Fenton-like catalyst to relieve the crisis. The transformation of Fe species at different carbothermal temperature was evaluated by XRD analysis. SEM and XPS analyses were involved to characterize the morphology and chemical bonds of the catalysts. Results shown that the resulted catalyst carbonized at 800 °C (Fe-SC-800) was composed of Fe0 and Fe3O4, performing nano-flake-like structure. The Fe-SC-800 has the highest catalytic activity in degradation of AOII in C0 = 200 mg/L. The efficiency achieves at 98% within 30 min at neutral pH, which is ascribed to the hydroxyl radical oxidation. Moreover, no iron is leached and the Fe-SC-800 could be recycled for three times at least. Thus, the Fe rich sludge could be reutilized as a valuable source for eco-friendly catalyst production, constituting an ecological way to manage these sludge wastes and eliminate the sludge and organic pollution to environment.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.