We show that dilute Al additions can control the size of primary Cu6Sn5 rods in Sn-0.7Cu/Cu ball grid array joints. In Sn-0.7Cu-0.05Al/Cu joints, the number of primary Cu6Sn5 per mm2 is ∼7 times higher and the mean three-dimensional length of rods is ∼4 times smaller than in Al-free Sn-0.7Cu/Cu joints, while the area fraction of primary Cu6Sn5 is similar. It is shown that epitaxial nucleation of primary Cu6Sn5 occurs on δ-Cu33Al17 or γ 1-Cu9Al4 particles, which are stable␣in the Sn-0.7Cu-0.05Al melt during holding at 250°C. The observed facet relationships agree well with previously determined orientation relationships between δ-Cu33Al17 and Cu6Sn5 in hypereutectic Sn-Cu-Al alloys and result in a good lattice match with <∼2.5% lattice mismatch on two different interfacial planes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.