Abstract

This work addressed on size control of WC grains in WC–FeAl composite fabricated from vacuum sintering techniques. Carbide additives and oxygen were candidates for the size controller of WC grains. The carbide additives such as VC and Cr3C2 suppressed the WC grain growth, which was similar to WC–Co system. As a result, they improved Vickers hardness, but degraded transverse rupture strength. On the other hand, some amount of oxygen included in the composite also suppressed the WC grain growth but improved both the hardness and the strength. It is concluded that oxygen is one of the most effective size controller of WC grains in the WC–FeAl system.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.