Abstract

The nitrogen concentration in liquid lithium was controlled by the hot-trap method. Titanium, vanadium and a V–Ti alloy were used as nitrogen gettering materials. Gettering experiments were conducted at 673, 773 and 823 K for 0.4–2.8 Ms. After immersion, the nitrogen concentration increased in titanium and V–Ti were tested at 823 K. Especially the nitrogen gettering effect by the V–10at.%Ti alloy was found to be large. Nitrogen was considered to exist mainly as solid solution in the V–10at.%Ti alloy. The decrease of the nitrogen concentration in liquid lithium by the V–Ti gettering was also confirmed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.