Abstract

The hardness and the structure of the heat-affected zone (HAZ) under welding of tube steels of strength category K60 – K70 are studied. The steels are treated by regimes imitating the thermal cycles of different welding processes applied to tubes starting with manual arc welding and ending with energy-intensive automatic submerged-arc welding. The welding modes causing maximum decrease in the hardness of HAZ regions are determined. The conditions preventing softening under one-pass and multipass welding of high-strength steels are presented.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.