Abstract

The electrospray deposition (ESD) method is an established film-forming technique. The pre-tilt angle was controlled by using the improved ESD method has been proposed by our previous report. In this paper, a novel torque balance method for measuring an improved azimuthal anchoring strength for the high pre-tilt angle was proposed. The pre-tilt angle was controlled and the azimuthal anchoring energy depended on the pre-tilt angle was evaluated. The azimuthal anchoring energy was obtained in the range from 10−4 to 10−5 J/m2 depending on the pre-tilt angle.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.