Abstract

CuO/γ-Al2O3 and CuO–MnO2–Fe2O3/γ-Al2O3 catalysts were synthesized by impregnation method. Their performances for selective catalytic reduction (SCR) were explored in a 200MW coal-fired power plant boiler tail flue. The effects of catalyst amounts, NH3/NO molar ratios, abrasion resistance, catalyst regeneration and the catalytic efficiencies for Hg0 oxidation were also discussed here. The optimum temperature range for the SCR of NO over fresh catalysts was 300~400°C. In the optimum temperature range, the efficiencies of the two catalysts were over 80%, with a maximum efficiency of nearly 90% obtained at 350°C. Reducing the catalyst amounts to half did not change the efficiency dramatically. The highest SCR activity was obtained with NH3/NO molar ratios ranging from 1.0 to 1.2. Abrasion resistance test indicates that the mechanical strength of the catalysts can bear the industrial scale and long-term erosion of fly ash. The activities of the catalysts remained constant during a 200h test. Meanwhile, the catalysts were able to maintain excellent NO reduction efficiency after three times recycling. CuO/γ-Al2O3 and CuO–MnO2–Fe2O3/γ-Al2O3 achieved 40% and 80% Hg0 oxidation efficiency, respectively. The present study provides a promising catalyst for NO and Hg0 removal for coal-fired power plants.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.