Abstract

A creep Deformation Mechanism Map (DMM) of an engineering alloy can be an effective tool for developing physics based prognostics systems. Many classical diffusion based rate equations have been developed for time dependent plastic flow where dislocation glide, dislocation glide-plus-climb and vacancy diffusion driven grain boundary migration (diffusion creep) are rate controlling. Long term creep testing and analysis of complex engineering alloys has shown that power law breakdown phenomenon is related to the dominance of Grain Boundary Sliding (GBS) as opposed to diffusion creep. Rate equations are now available for GBS in complex alloys and, in this paper, a DMM is constructed for Waspaloy (a Nickel-Based Superalloy) and validated by comparison with a collection of experimental data obtained from the literature. The GBS accommodated by wedge type cracking is considered dominant at low homologous temperatures (0.3 to 0.5Tm - temperature in Kelvin) whereas GBS accommodated by power-law or cavitations creep dominates above 0.55Tm.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.