Consolidation of flame hydrolysis deposition silica soot with a 9.3 µm CO2 laser has been demonstrated. A range of laser parameters were investigated and the surface roughness of the resulting silica layers were characterised with a stylus profiler and white light interferometer. The surface roughness parameters were Ra = 68.9 nm, Rq = 83.8 nm perpendicular to the trajectory of the translated laser beam for a speed of 300 mm s−1 and an average laser power of 42.5 W, and Ra = 29.5 nm, Rq = 36.18 nm along the trajectory of the translated laser beam for a speed of 250 mm s−1 and an average laser power of 35.8 W.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.