Abstract
We investigated energetics of binding of multifunctional pyranine ligands to hydrogels of the cross-linked poly(methoxyethylaminophosphazene) (PMOEAP) from data on the thermotropic volume phase transition of the gels by means of high-sensitivity differential scanning calorimetry. Dependences of the transition temperature, enthalpy, and width on the concentration of pyranines were obtained, and the excess transition free energy as a function of the pyranine concentration was calculated. We found that the affinity of the gels for the pyranine ligands increased very significantly upon the gel collapse. The intrinsic binding constants and free energies of binding of the ligands to the gels in the collapsed state were estimated from the DSC data. They revealed a significant increase in the hydrogel affinity for pyranines proportional to the number of anionic groups in the ligand structure. The affinity of the PMOEAP hydrogels for the multifunctional ligands was not affected by an increase in the cross-linking density of the gels and only slightly reduced by physiological salt concentrations.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have