Abstract

The non-asbestos organic friction materials with various abrasives such as ZrO2, ZrSiO4, Al2O3, Fe3O4 were manufactured and underwent friction tests to find conditions for transfer film formation and their effect on friction coefficients, and also the effect of different abrasive components was analyzed. Friction tests were composed of the effectiveness test and the fade & recovery test successively and counterpart disks were examined at each stage to find transfer film distribution changes. Friction surface observation by SEM revealed that the transfer film was formed not in the effectiveness stage which simulated the normal braking condition, but in the fade stage when temperature rose up to 600°C. The level of friction coefficients for most friction materials turned out to be opposite to the quantity of transfer film formation implying that the transfer film reduced the friction coefficient. High temperature condition was requisite for transfer film generation, but the transfer film was hardly formed irrespective of the magnitude of deceleration rate under moderate operating conditions where temperature stayed below 350°C. Among the friction materials tested, friction material which contained Al2O3 produced the least transfer film but showed the highest friction coefficient throughout the entire stages of the friction test.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.