Abstract
Mechanical behaviour of old masonry may differ from the theoretical one to a great extent, hence it needs to be properly evaluated for quantifying the safety and serviceability of real structures, in view of their rehabilitation and/or seismic reliability assessment. Among the factors affecting such behaviour, the presence of moisture, mainly from rising damp, plays a key role in the deterioration state of old masonry structures, owing to salt crystallisation, frost damage, etc. Besides, water presence in the material pores may also directly influence their mechanical properties (compressive and tensile strength, elastic modulus), due to the interactions with the pore surface, enhancement of crack propagation velocity and other mechanisms. Although the effect of water saturation has been investigated for clay-bearing rocks, ceramics and concrete, its consequences on the mechanical behaviour of brick masonry still requires in-depth elucidation. For this reason, in the present paper the compressive strength and Young’s modulus of fired-clay bricks, cement-based and lime-based mortars as well as masonry triplets are investigated, in dry and wet conditions. The results are interpreted in the light of the microstructural features of the materials, i.e., total voids amount and pores size distribution.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.