As a nickel-based alloy, GH4169 has the properties of excellent corrosion resistance, high temperature oxidation resistance and high creep resistance. In this paper, the compression creep behaviors of cylinder entangled wire materials (CEWMs) made from metal wires (GH4169 nickel-based alloy, 304 stainless steel) were investigated at elevated temperatures (from 400 °C to 500 °C). The performance degradation of the two materials was evaluated by the variation amplitude of four mechanical properties parameters and material characterization methods. The results indicated that both of 304 CEWMs and GH4169 CEWMs suffered a significant performance degradation at elevated temperatures, and both of the two CEWMs showed a much serious performance degradation above 450 °C (tempering temperature). Compared to the 304 CEWMs at the tested temperatures, the GH4169 CEWMs obtained better creep resistance. It is therefore concluded that the GH4169 CEWM is an excellent material that can replace the commonly used 304 CEWM at elevated temperature work conditions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.