Structural analysis was performed on the 55 kinds of diamond-like carbon (DLC) films. The ratio of sp 2 hybridized carbon in the film, sp 2/(sp 2 + sp 3) ratio, was determined by the carbon K-edge near-edge X-ray absorption fine structure (NEXAFS) spectroscopy using synchrotron radiation in the soft X-ray region. In addition, hydrogen content in the DLC film was determined by elastic recoil detection analysis (ERDA) using an electrostatic accelerator. Furthermore, the density of the DLC film was measured by X-ray reflectivity method. Analyzed DLC films were divided broadly into four groups. Group 1 was characterized by high density, low sp 2/(sp 2 + sp 3) ratio and low H content. Group 2 was characterized by low density, high sp 2/(sp 2 + sp 3) ratio and low H content. Group 3 was characterized by medium density, and medium sp 2/(sp 2 + sp 3) ratio and relative high H content. Most samples in the present study were belonging to this group. Group 4 was characterized by low sp 2/(sp 2 + sp 3) ratio in spite of low density. H contents of samples in this group were relatively high.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.