Abstract
Boron is known to influence the grain boundary microchemistry and thereby improve the mechanical performance of superalloys; however, the form in which boron exists at the grain boundary is debatable. We show from electron microscopy characterization that in a directionally solidified Ni-base superalloy boron is present in the form of nearly spherical nano-sized metal borides. We also report for the first time ever the existence of a gradient in composition of Cr, Mo and W within the nano-sized boride precipitates lying along the grain boundaries. These borides are present discretely and suppress the agglomeration of mostly reported M 23 C 6 carbides at the columnar grain boundaries. This could be a possible reason for the reported improvement in transverse creep properties of boron modified directionally solidified superalloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.