The influence of the composition of powder wire on the properties of the applied layer on steel samples is studied in the laboratory. If amorphous graphite in 35V9Kh3SF powder wire is replaced by material containing carbon and fluorine, the porosity of the applied layer is reduced, and fewer nonmetallic inclusions (including row oxide inclusions and undeformable silicates) are present. Statistical analysis of the experimental data illustrates the influence of the carbon equivalent of the 35V9Kh3SF powder wire on the hardness of the applied layer (including the mean surface hardness and the microhardness of martensite). With increase in the carbon equivalent calculated by the Paton Institute’s formula, the hardness of the applied layer linearly increases.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.