We investigated the effect of ternary shell alloy composition on the bandgap and diameter of core of ZnSe/Cd1−xZnxS heterostructure core/shell quantum dots, which were synthesized by using a simple colloidal technique. Characterization by using the x-ray diffraction (XRD), transmission electron microscopy (TEM), UV–Vis absorption and fluorescence emission spectroscopic techniques indicate that (i) there is a transition of ZnSe/Cd0.6Zn0.4S Type-I heterostructure (electrons and holes tend to localize in core) to ZnSe/Cd0.75Zn0.25S quasi-Type-II heterostructures (holes tend to localized in the core and electrons are delocalized) and (ii) then after large red shift and Stock-shift in PL emission spectra but not a distinct absorption peak in UV spectra become noticeable in ZnSe/Cd0.75Zn0.25 S quasi-Type II and ZnSe/CdS Type II heterostructures (electrons are localized in core and holes are localized in shell). Furthermore, the increase of Cd:S ratio in shell alloy composition shifts the XRD peaks to lower 2θ degrees which corresponds to tensile strain in the ZnSe core. Finally, the hydrostatic interfacial strain has effect on the squeezing or stretching the capped core: A decrease of compressive force on core from ZnSe/ZnS to tensile force in ZnSe/CdS with increase in Cd:S ratio indicates that transition of compressive strain to tensile strain takes place with the transition from Type-I to II heterostructure.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.