Thin films of ZnO0.7NiO0.3 have deposited on glass substrates at room temperature by using thermal evaporation technique under vacuum 10-5 mbar. The optical properties and dispersion parameters of the films have been studied. Changes in direct optical energy band gap of films were confirmed before and after annealing. The optical energy gap Eg decreased from 3.11 to 2.86 eV with increasing of annealing temperature to 200 °C. Some of the optical absorption parameters, such as optical dispersion energies Eo and Ed, Urbach tails EU , dielectric constant ε, the average values of oscillator strength So, and wavelength of single oscillator λo have been reported. An increase in the annealing temperature causes an increase in the average oscillator strength from 62.02 to 87.71 eV.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.