Aramid fibre, poly-m-phenylene isophthalamide (Teijin-Conex), was used to reinforce thermoplastic elastomer, styrene (ethylene butylene) styrene (SEBS). It was found that the moduli at 100 and 300% elongation of the composite increased linearly with increasing fibre loading. On the other hand, tensile strength of the composites decreased as the fibre content was increased. Improvement of interfacial adhesion was carried out by, first, slightly hydrolysing the fibre with sodium hydroxide solution to increase the number of reactive amino end groups and then mixing with the matrix and compatibiliser, maleic anhydride grafted SEBS (MA-g-SEBS), at various concentrations. Tensile strength of the compatibilised composite was found to increase and then level-off at 5 wt% compatibiliser. Fractured surface of composite containing compatibiliser showed more fibre breakage than the uncompatibilised one. Examination of the extracted fibre revealed that some fraction of rubber was chemically bonded to the fibre surface. These results suggest good compatibilising performance of MA-g-SEBS for the system studied.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.