Abstract

Abstract Complex material parameters (piezoelectric coefficient d31, elastic s11 E, and the dielectric constant K33) of the relaxor ferroelectric ceramic (1−x) Pb(Mg1/3Nb2/3)O3-xPbTiO3(x =.07) with 1% La (lanthanum) were measured as a function of bias field using a bar resonator. The values of the dielectric and piezoelectric phase angles are found to be comparable (i.e., around 0.04 for a d.c. bias field of 2.5 kV/cm), while the elastic phase angle is an order of magnitude smaller (0.001 for the same d.c. bias). For comparison of complex material parameters found from bar resonators, a sample in the form of a small disk is used to measure Poisson's ratio as well as the real components of the piezoelectric and elastic coefficients as a function of bias field.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.