Abstract

A purpose of the present study is to investigate the compatibility of SiC/SiC composite material and AlN ceramics with liquid metals. Corrosion behavior of materials could be affected by non-metallic impurities like nitrogen in liquid lithium. Another purpose of the present study is to control the concentration of nitrogen impurity by using getter materials and to study the effect of getter materials on compatibility with AlN. At 700K, all of the SiC/SiC specimens, except high purity specimen, were entirely broken down in liquid lithium. Even in this high purity specimen, many cracks were observed on the surface. On the other hand, in the case of SiC/SiC with Li17Pb83 at 773K, all of the specimens were not corroded. At 673K, impurity levels in AlN were changed in the case immersed in liquid lithium with getter materials. At 823K, impurities in AlN were attacked by lithium and the surface of it was locally peeled off. It was also observed that the getter material captured nitrogen.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.