Alumina-forming austenitic (AFA) steels were evaluated for the lead fast reactor application in static and flowing high-purity Pb. Two AFA composition ranges with different Ni, Mn, Al, Cr and Nb contents were targeted, and Zr foil was used in an attempt to getter O in some capsules. Based on two rounds of capsule testing at 500–800°C, two AFA compositions were selected for evaluation in flowing Pb with a peak temperature of 650°C in a thermal convection loop made of pre-oxidized FeCrAlMo tubing. After exposure for 1000 h, the mass losses for both AFA alloys were generally low, suggesting good compatibility under these conditions without preoxidation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.