Abstract
Indentation cracks are used as controlled flaws in soda-lime glass specimens for failure tests in uniaxial and biaxial loading. The inert strength is independent of loading type within the scatter of data. This result is discussed in relation to the conclusions of other workers who have reported systematic differences in similar comparative tests on specimens containing natural flaws.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Journal of the American Ceramic Society
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.