Abstract

Poor reactivity of fly ash (FA) in alkali activation process can be improved either by mechanical activation of fly ash or by blending fly ash with more reactive material, such as blast furnace slag (BFS). Both options were explored in this paper and comparison was performed. Mechanical activation of fly ash was conducted in a planetary ball mill, while blends of fly ash and blast furnace slag were prepared with different ratios (FA/(FA+BFS) = 1; 0.75; 0.50; 0.25; 0). Alkali activation was carried out at 95°C by use of sodium silicate solution as an activator. In both cases significant increase of geopolymer strength was observed in respect to the geopolymer based on the initial fly ash. Optimal geopolymer strength was correlated with the chemical composition of the binding gel. Empirical values of optimal gel composition could serve as a basis for tailoring properties of alkali-activated binders based on different precursors. Both alkali-activated systems represent promissing routes for geopolymer technology development.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.