Abstract

This paper reports the theoretical assessment of cracking which may occur when a severe cycle comprising alternate upshocks and downshocks is applied to an axisymmetric feature with an internal, partial penetration weld and crevice. The experimental observations of cracking are reported separately. A good agreement was noted even though extensive cycle plasticity occurred at the location of cracking. It is concluded that the LEFM solution has correlated with the experiment mainly because of the axisymmetric geometry which allows a large hydrostatic stress to exist at the internal weld crevice end. Thus the stress at the crevice can approach the singular solution required for LEFM correlations without contributing to yielding.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.