Sodium oleate (NaOL) and benzohydroxamic acid (BHA) are commonly used scheelite and cassiterite flotation collectors. Hydrophobic flocculation flotation of fine minerals has been extensively studied and reported under a NaOL system, but not under a BHA system. In this paper, the particle size distribution and flotation behaviour of fine scheelite (−10 μm) and cassiterite (−37 + 10 and −23 μm) after shear stirring in NaOL, BHA, and Pb2+ + BHA systems were studied by laser particle size analysis and flotation tests. The measured particle size distribution results revealed that the fine minerals could aggregate under a NaOL system, and the aggregate size increased with increasing stirring time and speed, with scheelite aggregating faster than cassiterite. BHA did not cause scheelite or cassiterite to form hydrophobic aggregates. At low stirrer speeds, the minerals could form small, weak, and easily broken aggregates when Pb2+ + BHA was added. The results of the flotation tests revealed that increasing the stirring time and speed increased the flotation rate and recovery when NaOL and BHA were added. When Pb2+ + BHA was added, however, the changes in flotation rate and recovery were not noticeable when the stirring conditions were changed.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call