ZnO thin films have been deposited by pulsed laser deposition (PLD) and ultrasonic spray pyrolysis (USP) method, respectively. X-ray diffraction and transmission electron microscopy characterizations indicate that ZnO film grown by PLD exhibits better crystallinity than that grown by USP. Photoluminescence spectra show that the near-band edge ultraviolet emission of film grown by PLD is narrower and shifts to higher energy, compared with that of film grown by USP. In the visible range, ZnO film grown by PLD exhibits four local level emission centered at 470 nm, 486 nm, 544 nm, and 613 nm, respectively, while the film grown by USP only presents a weak broad band emission centered at 502 nm. Hall measurement shows higher carrier density and lower hall mobility in ZnO film grown by PLD than that in film grown by USP. The higher density of intrinsic defects as well as higher crystallintiy is considered to account for the difference of photoluminescence in ZnO film grown by PLD with that in film grown by USP.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.