Abstract

To compare the 2-year success rates of a Resin Modified Glass Ionomer Cement (RMGIC) with a composite resin in class II primary molar restorations. Healthy, cooperative children aged 4-7.5years with at least one carious primary molar requiring a class II restoration were included in this parallel randomised trial and allocated on a 1:1 basis to composite resin (Z250, 3M ESPE) or RMGIC (Vitremer, 3M ESPE). Restorations were assessed semiannually up to 2years clinically and radiographically using modified United States Public Health Service criteria, with the primary outcome being all-cause failure. Data were analysed per protocol by binomial linear regression with Relative Risks (RR) and their 95% confidence intervals (CI). 55 patients were randomly allocated to either group and 44 analysed at 2 years; with 49 teeth in the Z250 and 55 teeth in the Vitremer group. The all-cause failure rate for both materials was 3% after 1year (4 and 2% for Z250 and Vitremer, respectively) and 16% after 2years (16% for both Z250 and Vitremer). Overall, no difference between materials could be found at 2years (RR = 1.4; 95% CI 0.8, 2.4; P = 0.30). However, Vitremer was associated with more favourable gingival health compared to composite (RR = 0.2; 95% CI 0.1, 0.9; P = 0.03), but also occlusal wear, which was observed exclusively for Vitremer. No significant difference was found in the overall performance of the two materials, making them suitable for class II primary molar restorations, although RMGIC presented more pronounced occlusal wear of limited clinical importance after 2years.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call