Abstract

The 2 mm sheet of 6082 - T6 aluminum alloy was carried to develop refill friction stir welding and withdrawing friction stir spot welding,the forming of solder joints , the cross-sectional microstructure and fracture morphology of welding joints were observed and analyzed, the cross-sectional microhardness of welding joints were tested. Tensile shear load and fracture mode were contrasted simultaneously. The results showed that smooth surface and free of macroscopic defects of welding joints could be obtained in both welding type. Tensile shear load of WFSSW was up to 10.28kN under the optimal process parameters greater than RFSSW’s 8.62kN.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.