Abstract

ABSTRACTA number of F2-based plasma chemistries (NF3, SF6, PF5 and BF3) were investigated for high rate etching of SiC. The most advantageous of these is SF6, based on the high rate (0.6 μm · min−1) it achieves and its relatively low cost compared to NF3. The changes in electrical properties of the near-surface region are relatively minor when the incident ion energy is kept below approximately 75 eV. At a process pressure of 5 mTorr, the SiC etch rate falls-off by ∼15 % in 30 μm diameter via holes compared to larger diameter holes (> 60 μm diameter) or open areas on the mask.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.