AbstractPolyacrylonitrile (PAN) hollow fibers were pretreated with five different compounds containing phosphorus, including ammonium dibasic phosphate, ammonium dihydrogen phosphate, triammonium phosphate, phosphoric acid, and metaphosphoric acid, and then further oxidized in air, carbonized in nitrogen, and activated with carbon dioxide. The effects of different compounds containing phosphorus as pretreating agents on the properties and structure of the resultant oxidized hollow fibers, carbon hollow fibers, and activated carbon hollow fibers are discussed. Comparing the Brunaner‐Emmett‐Teller (BET) surface area of PAN‐activated carbon hollow fibers (ACHF) pretreated with five different compounds, ammonium dibasic phosphate > triammonium phosphate > ammonium dihydrogen phosphate > phosphoric acid > metaphosphoric acid, and the surface area of mesopores in PAN‐ACHF pretreated with ammonium dibasic phosphate reaches maximum, 174 m2 g−1. The adsorption ratio to mesomolecule adsorbate, VB12, of PAN‐ACHF pretreated with ammonium dibasic phosphate also reaches maximum, 97.7 wt %. Moreover, the dominant pore sizes of PAN‐ACHF range from 2 to 5 nm in diameter. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 96: 294–300, 2005

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.