Abstract
<p>An experimental investigation was carried out to compare the compressive strength of zero slump and high slump concrete with high volume fly ash. 40% to 70% replacements of OPC (by weight) with class F fly ash have been incorporated. Superplasticizer was added at 1% of binder (cement + fly ash) to the zero slump mixture to get a slump in the range of 140 to 180mm and cubes were cast without compaction. The results showed that the apparent porosity and water absorption were higher for zero slump concrete than high slump concrete. Zero slump concrete showed better compressive strengths than superplasticized concrete with 40 to 60% fly ash addition for all curing times tested (3,7 and 28 days). Ultrasonic pulse velocity results categorized all mixes as of &lsquo;EXCELLENT&rsquo; concrete quality. Based on the present experimental investigation, it can be concluded that high volume fly ash concrete is suitable for general construction applications.</p>
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.