Abstract

AbstractGold nanoparticles where synthesized and supported on carbon, or directly synthesized on carbon according to five different methods reported in literature, aiming at particles<10 nm. Characterization was done with transmission electron microscopy and thermogravimetric analysis. Although all syntheses yielded particles with an average diameter<10 nm, the formation of few very large particles, where a relatively large amount of Au is buried, as well as loss during the supporting procedure led to the exclusion of four of the five tested methods for further studies. The most promising AuNPs supported on carbon where tested for the methanol electrooxidation (MEO) in alkaline media. Four different Au‐loadings where realized, and supporting led to moderate particle growth depending on the loading. To compare MEO activity of the samples with different Au‐loadings a conversion factor was developed where the MEO activity can be compared in terms of NP size and Au‐loading.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.