Chemical solution deposition (CSD) techniques were used to prepare lead zirconate (Zr) titanate (Ti) (PZT) thin films with Zr/Ti ratios of 30/70 and 52/48. Usually CSD processing is restricted to making crack-free, single-layer films of 70-nm thick, but modifications to the sol-gel process have permitted the fabrication of dense, crack-free, single layers up to 200 to 300 nm thick, which can be built-up into layers up to 3-microm thick. Thicker PZT films (> 2-microm single layer) can be produced by using a composite sol-gel/ceramic process. Knowledge of the electroactive properties of these materials is essential for modeling and design of novel micro-electromechanical systems (MEMS) devices, but accurate measurement of these properties is by no means straightforward. A novel, double-beam, common-path laser interferometer has been developed to measure the longitudinal (d33) piezoelectric coefficient in films; the results were compared with the values obtained by Berlin-court and laser scanning vibrometer methods. It was found that, for thin-film samples, the d(33,f) values obtained from the Berlincourt method are usually larger: than those obtained from the interferometer and the vibrometer methods; the reasons for this are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IEEE Transactions on Ultrasonics, Ferroelectrics and Frequency Control
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.