Abstract

Aim: The aim of this study was to evaluate and compare the compressive strength, Vickers microhardness number, and wear resistance of amalgam (DPI), Filtek Z350 nanohybrid (3M ESPE), and Zirconomer (Shofu) restorative materials after 24 h and 3 months. Methodology: The restorative materials were divided into Zirconomer (Group I), Filtek Z350 (Group II), and amalgam (Group III). These materials were placed in cylindrical molds to prepare the specimens. The specimens were stored in distilled water at 37°C. The specimens were tested at 24 h and 3 months for compressive strength, wear resistance, and microhardness. Results: Group I showed significantly less maximum load (N) and compression strength (MPa) when compared with Group III (control) and Group II (P < 0.01). There was no significant difference in microhardness between the three groups. Group I showed significantly more wear (weight loss [g]) and wear (weight loss [%]) when compared with Group III (control) and Group II. Conclusion: The study concludes that amalgam and nanohybrid composite performed better than Zirconomer at the end of 24 h and 3 months.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.