Two methods, HCl and enzymatic treatments, were evaluated for diversification of morphological and functional properties of cellulose nanofibers (CNF) from two- stage-alkaline pre-treated wheat straw (WS). The extraction conditions were optimized by a central composite designed experimental approach varying time (4–8 h) and temperature (80–120 °C) for the HCl-based treatment and time (4–8 h), and FiberCare dosage (50–100 endo-1,4-β-glucanase unit/g) and Viscozyme (10–20 fungal β-glucanase units/g) for the enzyme-based treatment. The CNF yields, morphological (polydispersity index (PdI), length and diameter), and functional (crystallinity and thermal degradation) properties were compared. The CNF produced by the HCl (HCN) and enzymatically (ECN) attained diameters ~17 nm had PdI, length, and crystallinity of 0.53, 514 nm & 70%, and 0.92, 1.0 μm & 48%, respectively. Thus, the HCN morphology suits homogenous nano-applications, whereas that of the ECN, would suit heterogenous nano-applications. The HCN and ECN yields were similar (~20%) with optimal production time of 7.41 and 4.64 h, respectively. Both the HCN & ECN can be classified as thermally stable nanocolloids with maximum thermal degradation temperatures of ~380 °C and Zeta potential ~-16 mV. The two CNF production methods have potential synergetic effects on CNF production, morphological, and functional properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.