When bulk ferromagnetic Fe80P13C7 amorphous rods of approximately 2-mm diameter are compacted together in a hot press, a variety of different microstructures, depending on the experimental conditions, are produced. The most intriguing microstructure is that two different bulk amorphous rods can be fused together perfectly at a temperature of 683 K and under a pressure of 2.5 to 4 GPa for a period of 5 min.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.