Abstract

The comminution of a typical submicrometre B4C powder with a high-energy mill (i.e., a shaker mill) operated in air in either a dry or a wet environment was investigated. It was found that dry shaker milling (i.e., high-energy ball-milling) is able to progressively refine the B4C particles to the nanoscale. While this is accompanied by oxidation and aggregation, these are not serious drawbacks. Wet shaker milling in methanol (i.e., conventional ball-milling) resulted only in a moderate B4C particle refinement with greater contamination by the milling tools, which limits its usefulness. It was also found that both dry and wet milling modify the B4C crystal structure, attributable to carbon enrichment. Consequently, dry shaker milling was found to be more recommendable than wet shaker milling to provide B4C starting powders with superior sinterability. A comparative densification study by spark-plasma sintering confirmed this recommendation, and also showed the usefulness of dry shaker milling to obtain refined B4C microstructures for structural applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.