Abstract
Li8Bi2(MoO4)7 was synthesized by a one-step combustion method. The structure, morphology, adsorbance, optical and photocatalytic properties of as-obtained sample were studied by X-ray powder diffraction, scanning electron microscopy, ultraviolet–visible spectrophotometry. The experimental results show that the formation of tetragonal Li8Bi2(MoO4)7 was one-pot achieved. The sample exhibits a irregular particle morphology with an average size of ~0.6μm. The direct energy band gap calculated from the diffuse reflectance spectrum is 3.25eV. Compared with TiO2 (P25), as-synthesized Li8Bi2(MoO4)7 shows better visible light photodegradation performance for MB, which can be attributed to its excellent adsorbability.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.