Abstract An unique com-shaped silicone-alkyd resins (SiAR) were synthesized with high solid content (65 wt%) prepared from an alkyd resin (AR) and a varying weight% (5, 10, 15, 20) of silicone moiety (Z-6018) by etherification reaction. The viscosity and the hydroxyl value (OHV) of the SiAR were found to be higher than those of the AR. The formation of the SiAR was confirmed by infrared spectroscopy and mass spectrometry analysis. The glass transition temperature (T g ), thermal stability, and molecular weight of the SiAR, increased with increasing the silicone content and compared with those of the AR. The results of chemical resistance showed that the SiAR exhibited a better resistance than AR against 0.1 M sodium hydroxide (NaOH) solution.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.