Abstract

Metal dissolution from tailings collected at a gold-copper mine mill site was examined by researchers from the U.S. Bureau of Mines using column leaching procedures and on-site field monitoring wells. The 3-year laboratory study reviewed effects of column waste depths, dry cycles, waste sampling locations, and metal dissolution abatement techniques. Results of the laboratory testing indicated that the concentrations of metals in the leachate gradually decreased with each leaching and that metal release from unsaturated tailings was enhanced in most, but not all, samples. Sulphide-rich tailings produced leachates with a pH in the range of 2 to 4, sulphate concentrations as high as 40,000 mg/L, and copper concentrations in the range of 0.2 to 2,400 mg/L. The effects of abatement treatments using phosphate, lime, and sodium lauryl sulphate were also examined, but the treatments were demonstrated to be of only marginal value. The interaction between tailings and wood chips, and tailings and a compost-peat moss mixture was also studied.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.