ABSTRACTEpitaxial La0.67Ca0.33MnO3(LCMO) films have been grown by pulsed laser deposition technique on three single crystal substrates: LaAlO3, SrTiO3, and NdGaO3 having lattice mismatch with LCMO film of + 1.26 %, - 0.9 %, and + 0.18 %. We found the transport colossal magnetoresistive (CMR) properties were improved with the reduction of a film/substrate mismatch. Processing conditions for LCMO film on NdGaO3substrate were optimized as well as post-annealing process was employed to achieve a superior temperature coefficient of resistivity TCR = 35 %K−1 and the magnetoresistance MR = 66 % at 7 kOe. To our knowledge, these are the record CMR parameters achieved so far.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.