Abstract

Color changes of ash wood (Fraxinus excelsior L.) caused by thermal modification in air and steam. Ash wood samples of 20x20x30 mm were subjected to thermal modification in different conditions. The thermal modification was conducted in air at 190 °C and in steam at 160 °C. For both environments modification lasted 2, 6 and 10 hours. Samples color parameters were measured before and after thermal modification on the basis of the mathematical CIELab color space model. Changes in all parameters (L, a and b) were observed, the highest in lightness (L) - darker color. The total color difference (ΔE) and chromaticity change (ΔC) were calculated for all samples. The highest value of ΔE was obtained for wood modified in the air at 190 °C for 10 h. The highest value of ΔC was obtained for wood modified in steam at 160 °C for 10 h. However, the value obtained for wood modified in the air at 190 °C for 10 h were only slightly lower.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.