Abstract

Much chromite ore processing residue (COPR), which is defined as hazardous solid waste due to virulent Cr (Ⅵ), is produced from chromium salt industry. C-bearing dust from steel industry is a kind of typically solid waste with poor surface activity. The iron ore sintering process has the potential on large-scale harmless utilization of COPR and C-bearing dust. This study proposes a new approach of co-utilizing COPR and C-bearing dust during limonitic laterite sintering process. The negative influence of COPR and C-bearing dust on permeability was offset by the fuel attribute of extra C from C-bearing dust. The results indicate that, while 6% COPR and 8% C-bearing dust were added, the tumble index and yield of the sinters were basically equal to those of the blank samples. The toxic Cr (Ⅵ) was reduced to Cr (Ⅲ) which was concentrated in high alumina spinel phases during the sintering process. The obtained sinters were identified as nontoxic, and no secondary waste was generated throughout the clean utilization process.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call