Abstract
Low-density polyethylene (LDPE) and polylactic acid (PLA) plastic films were subjected to modification using different plasma sources. Argon, nitrogen, air and oxygen were used as a gas phase throughout the process, and their impact on the material's surface properties was verified. The surface activation rate was measured via atomic force microscopy regarding the porosity factor and using the water contact angle technique. The last method – being feasible, agile and of high sensitivity to alternating physicochemical surface character – was utilised to verify the post-process stability of the modified surface. Those tests were performed extensively, up to 160 hours (contact angle) and 240 hours (atomic force microscopy).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.