Abstract
To efficiently co-extract Ni and Cu from low-grade nickel-copper sulfide ore, chlorination roasting with NH4Cl followed by a water leaching process was investigated. The results show that 98.4% Ni and 98.5% Cu can be synchronously extracted when the ore particle size is 75-80 μm, the roasting time is 2 h, the mass ratio of NH4Cl to ore is 1.6:1 and the roasting temperature is 550 °C. The evolution behavior of various minerals was elucidated using X-ray diffraction (XRD) coupled with scanning electron microscopy (SEM). The kinetics of the chlorination process based on the differential thermal and thermogravimetric analysis (DTA-TG) data was analyzed by Kissinger method and Flynn-Wall-Ozawa (FWO) method. The chlorination process of low-grade nickel-copper sulfide ore mainly contains two stages: the decomposition of NH4Cl and the chlorination of ore. The maximum apparent activation energies (Ea) at two stages are determined to be 114.8 and 144.6 kJ/mol, respectively. The condensed product of exhaust gas is determined to be ammonium chloride, which can be recycled as the reactant again, making the process economic and clean.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of Nonferrous Metals Society of China
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.