Abstract

Anisotropic ultrafine-grained Nd-Fe-B magnets with WC addition were prepared by hot deformation. With WC nano-particles addition of ~1.0wt.%, the squareness was optimized and the coercivity of the hot-deformed magnets increased substantially by 2.16kOe, from 15.59 to 17.75kOe without expense of the remanent magnetization. The observation for microstructure revealed that the WC nano-particles mainly existed on the interfaces of melt-spun ribbons. Meanwhile, due to the local compressive stress induced by the hard WC nano-particles, the deformability of neighboring grains was remarkably enhanced which leads to the reduction of the coarse grain regions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.