The purpose of this qualification work is to study the physical and mechanical behavior of concrete with the addition of 0.5% and 1% coconut fiber, which has been subjected to two chemical treatments to reduce its degradation. The coconut fibers were extracted from the raw material and cut into pieces 4 cm long. Subsequently, the fibers were subjected to two chemical treatments. The first involved immersing the fibers in 4% sodium hydroxide (NaOH) solution, and the second treatment involved coating them with gum arabic and silica fume. A total of 50 samples of fibers were collected in their natural and post-treated state to be tested. The dosage was prepared for design strengths of 210 and 240 kg/cm2 (20.59 and 23.54 MPa), so that the percentages of 0.5% and 1% volume of coconut fiber, for the two treatments selected, replaced the respective volume of coarse aggregates. The cylinders with 1% addition of fibers had the best performance for the design strength of 20.59 MPa, including the cylinders without fibers. Those with 0.5% addition of fibers presented better performance for the 23.54 MPa dosage, although this was lower than the cylinders without fibers. In all cases, the cylinders with NaOH-treated fibers outperformed their counterparts with fibers treated with gum arabic and silica fume. Finally, a CO2 balance was determined, and an environmental gain up to 14 kg in CO2 emissions was established for each cubic meter of composite concrete.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call